ISHYAKA RYA CHIMIQUE:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
AMATEGEKO ya GB / T. | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
AWS AMATEGEKO | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
URUGERO AGACIRO | 0.028 | 0.95 | 0.80 | 24.4 | 13.1 | 0.32 | 0.027 | 0.004 | 0.050 |
UMUTUNGO W'IKORANABUHANGA:
UMUTUNGO | IMBARAGA YIELD (MPa) | IMBARAGA ZIKURIKIRA (MPa) | GUSHYUSHA ℃ xh | AGACIRO KIDASANZWE J / ℃ | KUBONA (%) | |||||
AMATEGEKO ya GB / T. | - | 510 | - | - | 25 | |||||
AWS AMATEGEKO | - | 520 | - | - | 30 | |||||
URUGERO AGACIRO | - | 590 | - | - | 38 |
BASABWE PARAMETERS WELDING:
DIAMETERS UMWIHARIKO (mm) | 2.0 * 250 | 2.6 * 300 | 3.2 * 350 | 4.0 * 350 | 5.0 * 350 | |||||
AMATORA (Amp) | H / W. | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O / W. | 20-50 | 45-80 | 70-110 | 90-135 |
Inkunga y'uruganda
Igicuruzwa kibereye a
Ubwoko bwa Porogaramu
IKORANABUHANGA
Shaanxi Pucheng -50 ℃ propane spherical tank umushinga
Guangxi Huayi methanol dehydrating umunara
85000 m3 Imodoka nini cyane ya Ethane Vinyl (VLEC)
ISHYAKA RYA CHIMIQUE:
ALLOY (wt%) | C | Mn | Si | Cr | Ni | Mo | P | S | Cu |
AMATEGEKO ya GB / T. | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
AWS AMATEGEKO | 0.04 | 0.5-2.5 | 1.00 | 22.0-25.0 | 12.0-14.0 | 0.75 | 0.040 | 0.03 | 0.75 |
URUGERO AGACIRO | 0.028 | 0.95 | 0.80 | 24.4 | 13.1 | 0.32 | 0.027 | 0.004 | 0.050 |
UMUTUNGO W'IKORANABUHANGA:
UMUTUNGO | IMBARAGA YIELD (MPa) | IMBARAGA ZIKURIKIRA (MPa) | GUSHYUSHA ℃ xh | AGACIRO KIDASANZWE J / ℃ | KUBONA (%) | |||||
AMATEGEKO ya GB / T. | - | 510 | - | - | 25 | |||||
AWS AMATEGEKO | - | 520 | - | - | 30 | |||||
URUGERO AGACIRO | - | 590 | - | - | 38 |
BASABWE PARAMETERS WELDING:
DIAMETERS UMWIHARIKO (mm) | 2.0 * 250 | 2.6 * 300 | 3.2 * 350 | 4.0 * 350 | 5.0 * 350 | |||||
AMATORA (Amp) | H / W. | 50-75 | 70-95 | 80-120 | 110-160 | 160-190 | ||||
O / W. | 20-50 | 45-80 | 70-110 | 90-135 |